Pacific Code |
Composition |
Pressing Method |
Residual magnetic flux density Br (G) |
(Induction) Coercive force HcB(Hc) (Oe) |
Intrinsic coercive force HcJ(iHc) (Oe) |
Max
energy product B H max (MGOe) |
PMP- WAH |
SrO· 6Fe2O3 |
Wet-type anisotropic |
4,100∼ 4,300 |
2,700∼ 3,000 |
2,700∼ 3,100 |
4.0∼ 4.4 |
PMP- WAL |
SrO· 6Fe2O3 |
Wet-type anisotropic |
3,600∼ 4,000 |
3,100∼ 3,800 |
3,100∼ 5,000 |
3.2∼ 4.2 |
PMP- DAH |
SrO· 6Fe2O3 |
Dry-type anisotropic |
3,800∼ 4,100 |
2,800∼ 3,100 |
2,900∼ 3,200 |
3.5∼ 4.0 |
PMP- DAL |
SrO· 6Fe2O3 |
Dry-type anisotropic |
3,600∼ 3,800 |
3,200∼ 3,500 |
3,300∼ 3,600 |
3.0∼ 3.6 |
Pacific Code |
Green density (g/㎤) |
Sintered density (g/㎤) |
Shrinkage of diameter (%) |
Average particle diameter (㎛) |
PMP-WAH | 2.8∼3.0 | 4.9∼5.1 | 13.0±0.5 | 4∼6 |
PMP-WAL | 2.8∼3.0 | 4.8∼5.0 | 13.0±0.5 | 4∼6 |
PMP-DAH | 2.7∼2.9 | 4.8∼5.0 | 13.5±0.5 | 0.7∼1.0 |
PMP-DAL | 2.7∼2.9 | 4.8∼5.0 | 13.5±0.5 | 0.7∼1.0 |