Curie Point | 850∼890℃ |
Maximum Permissible Temperture | 550℃ |
Specific Resisitivity | 50∼75μΩ-㎝ |
Density | ∼7.3g/㎤ |
Hardness | Hrc45∼60 |
Thermal Expansion Coefficient | 11∼13.5×10-6/℃ |
Temperature Coefficient | - 0.016%/℃ |
Pacific Code | Residual Flux Density | Coercive Force | Maximum Energy Product | |||
Br | HcB(Hc) | (BH)Max. | ||||
kG | T | Oe | kA/m | MGOe | kJ/㎥ | |
PMC-1A | 12.3∼12.8 | 1.23∼1.28 | 650∼700 | 51.7∼55.7 | 5.0∼5.5 | 39.8∼43.8 |
PMC-1B | 12.5∼13.0 | 1.25∼1.30 | 600∼660 | 47.7∼52.5 | 4.8∼5.5 | 38.2∼43.8 |
PMC-1D | 12.8∼13.2 | 1.28∼1.32 | 650∼700 | 51.7∼55.7 | 5.3∼6.2 | 42.2∼49.3 |
PMC-1L | 11.8∼12.4 | 1.18∼1.24 | 570∼620 | 45.4∼49.3 | 4.5∼5.2 | 35.8∼41.4 |
HIMAG | 13.0∼14.0 | 1.30∼1.40 | 700∼800 | 55.7∼63.7 | 6.5∼8.0 | 51.7∼63.7 |
PMC-2B | 10.0∼11.0 | 1.00∼1.10 | 700∼780 | 55.7∼62.1 | 3.5∼4.2 | 27.8∼33.4 |
PMC-2C | 11.0∼11.8 | 1.10∼1.18 | 680∼750 | 54.1∼60.0 | 3.5∼4.5 | 27.8∼35.8 |
PMC-4A | 6.0∼7.0 | 0.60∼0.70 | 550∼620 | 43.7∼49.3 | 1.3∼1.6 | 10.3∼12.7 |
PMC-4B | 6.0∼7.0 | 0.60∼0.70 | 500∼550 | 39.8∼43.7 | 1.3∼1.5 | 10.3∼11.9 |
PMC-4C | 5.0∼6.0 | 0.50∼0.60 | 650∼750 | 51.7∼60.0 | 1.3∼1.7 | 10.3∼13.5 |
PMC-5AB | 8.0∼9.5 | 0.80∼0.95 | 130∼190 | 10.3∼15.1 | - | - |
PMC-8B | 8.3∼9.0 | 0.83∼0.90 | 1380∼1550 | 110∼123 | 4.8∼5.4 | 38.2∼43.0 |
PMC-8C | 8.5∼9.0 | 0.85∼0.90 | 1500∼1650 | 119∼131 | 5.0∼6.5 | 39.8∼51.7 |
PMC-8E | 7.5∼8.5 | 0.75∼0.85 | 1800∼2100 | 143∼167 | 5.5∼7.0 | 43.8∼55.7 |
PMC-9B | 10.0∼11.0 | 1.00∼1.10 | 1300∼1500 | 104∼119 | 9.0∼11.0 | 71.6∼87.5 |